Atomic layer deposition assisted fabrication of insertable silver dendrites-based SERS substrates with high adhesion

Xinxin Wang, Lin Zhu, Jisong Qian, Xiaoxiong Wang, Jianli Jiang, Aidong Li, Liyong Jiang*, Yanqiang Cao*

*Corresponding author for this work

Research output: Contribution to journalJournal articlepeer-review

2 Citations (Scopus)

Fingerprint

Dive into the research topics of 'Atomic layer deposition assisted fabrication of insertable silver dendrites-based SERS substrates with high adhesion'. Together they form a unique fingerprint.

Engineering & Materials Science

Physics & Astronomy